Effect OF Film Thickness And Annealing Time on Structural And Optical Propertieis Of The Oxides (Fe2030, Co304) And Their Mixtures
Keywords:
Spray deposition, Thickness, Iron, Cobalt.Abstract
Thin film technology is one of the most important technologies
that have contributed to the development of semiconductors and their
applications in several industrial fields. The Iron Oxides (Fe20) and
(Co3O4) thin films and their applications are of importance, in that these
two materials are considered as important industrial materials, and used
in spectrally selective coating, temperature sensors, resistive heaters, and
photo cells.
Thin films of Iron Oxide (Fe20,), Cobalt Oxide (Co304) and
their mixtures in different ratios (75:25, 50:50, 25:75) were prepared by
the method of chemical spray pyrolysis deposition at different thicknesses
(77s t S200) nm on cover-glass substrates: thickness of (1) mm at
temperature (653)OK, and at temperature (753)oK for (one, and two) hour.
The nature of the thin-films
surfaces are examined by optical
microscopy, while the crystallinity of the compounds is examined by X
ray diffraction (XRD)
The results of KRD) have shown that the films of (Fe20,) and
(Co304) and their mixtures are of amorphous structure. Annealing
operations led to transition of the films' structure from the amorphous to polycrystalline state. These obtained results were found in
agreement with the American Standard for Testing Materials (ASTM).
Film thickness, and annealing time were investigated, the results show the
crystallite size increases with the increase of the thickness of the thin
film
The increase in the annealing time for more than one hour resulted
in the appearance of some peaks in diffraction spectrum of the prepared
films. This verifies that it is polycrystalline, and this increases the time to
organize itself in the crystalline lattice and decreases the crystalline
defect. This research also included the study of the optical properties of
the prepared samples by recording the absorption and transmission
spectrum over the spectral range (200-900 nm, the optical energy gap for
the allowed direct transition was evaluated. In general, the optical energy
gap decreases with increase of the film thickness percentage of (Co3O4)
in the sample, and it increases after annealing
The optical parameters are investigated and calculated such a
optical absorption coefficient, photon energy, and the width of localized
states too. It is found that the values of absorption coefficient the
increases with increasing percentage of (Co3O4)